Jingyida PET Preform Mould Factory|Made in China Plastic Commodity Mould Suppliers|Preform Mold Make|Injection Molding Packaging Solutions

PET PREFORM MOLUD/PET BLOWING BOTTLE MOULD SUPPLIER FACTORY

Reasons and treatment methods for whitening of PET bottle embryo bottom

Cause analysis:

1. Insufficient drying of raw materials
2. The temperature of the mold diversion channel is too low
3. Insufficient cooling of the mold cavity
4. Adhesive glue looseness too low
5. The injection speed is too low

resolvent:

1. Check if the drying hopper is functioning properly, increase the drying temperature appropriately, and extend the drying time
2. Appropriately increase the temperature of the mold diversion channel
3. Check if the cooling water in the mold cavity is flowing smoothly
4. Adjust the looseness appropriately
5. Increase the injection speed